Mechanical Properties Metric English Comments
Flexural Modulus 9.55 - 18.6848 GPa

@Temperature -40.0 - 120 °C
1390 - 2710.04 ksi

@Temperature -40.0 - 248 °F
Average value: 15.7 GPa Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..