Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 274 GPa @Temperature 23.0 °C |
39700 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M60J Fiber Information provided by HexCel |