Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Resinoid 1340 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00DS PA 6 (Europe-Africa-Middle East) LNP THERMOCOMP* PF00DS is a compound based on PA6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy Rogers electrical encapsulation grade epoxy is recommended for capacitors, resistors, gold lead encapsulation, relays, coils and bobbins.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, DRY Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA6.6 (Europe-Africa-Middle East) LNP Verton* RV00CESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 19.03 GPa | 2760 ksi | ASTM D790 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | DIN 53 457 |
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |