Polymer Property : Flexural Modulus = 2890 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 19.9 GPa
2890 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data ..
Flexural Modulus 19.9 GPa
2890 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.
Flexural Modulus 19.9 GPa
2890 ksi
ASTM D790
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Flexural Modulus 19.9 GPa
2890 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 19.9 GPa
2890 ksi
GB/T 9341-2008
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Modulus 19.9 GPa
2890 ksi
ASTM D790
Plenco 1510 Polyester, Granular, Transfer Molded
PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file ..
Flexural Modulus 19.9 GPa
2890 ksi
Conditioned; ASTM D790
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..