Mechanical Properties Metric English Comments
Flexural Modulus 3.12 GPa
453 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 500ECR PC
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Flexural Modulus 3.12 GPa
453 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Flexural Modulus 3.12 GPa
453 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East)
Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a..
Flexural Modulus 3.12 GPa
453 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK
LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant.
Flexural Modulus 3.12 GPa
453 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS
LNP THERMOCOMP* NF001 is a compound based on PC+ABS resin containing 5% Glass Fiber.
Flexural Modulus 3.12 GPa
453 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS
LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber.
Flexural Modulus 3.12 GPa
453 ksi
ISO 178
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix
HexPly® 924 is a controlled flow epoxy matrix developed for the fabrication of high temperature resistant primary structures. When cured, HexPly® 924 becomes a tough composite with high impact res..
Flexural Modulus 3.12 GPa
453 ksi
50%RH; ISO 178
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform..