Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Resin, RT, Dry; ASTM D6272 |
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg. Straightforward 350°F Cure Designed for the unique requirements of satellite and missile structuresLow shrinka.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Resin, RT, Wet |
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 6781 S2 Glass Fabric RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg. Straightforward 350°F Cure Designed for the unique requirements of satellite and missile structuresLow shrinka.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM Data |
BASF Capron® 8200CQ Blend Nylon 6 (Dry)
(discontinued **) Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistanc.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.17 GPa @Temperature 23.0 °C |
459 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene GP150 Polystyrene APPLICATIONS: INJECTION MOULDING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARE, etc. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX200R PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Techmer ES Luriblend® POM HO TL10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5101-15 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding .. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Videolar 500 Crystal Polystyrene (GPPS) Designed for injection moldingVery easy flowing grade for fast cycle injection moldingExcellent processability for filling thin partsFeatures: Good strengthGood temperature resistanceExcellent clari.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | |
Asahi Kasei Thermylene® P-30TC-1156 Chemically Coupled Polypropylene Compound, 30% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled