Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0226 GPa | 3.27 ksi | ASTM D790 |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Flexural Modulus | 0.0226 GPa | 3.27 ksi | ASTM D790 |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |