Mechanical Properties Metric English Comments
Flexural Modulus 3.41 GPa
495 ksi
Flexural 0.5% Secant Modulus; ASTM D790
Greene Tweed ARâ„¢ HT Abrasive-Resistant Thermoplastic
ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outs..
Flexural Modulus 3.41 GPa
495 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Flexural Modulus 3.41 GPa
495 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific)
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Flexural Modulus 3.41 GPa
495 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 (Asia Pacific)
LNP* THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa..
Flexural Modulus 3.41 GPa
495 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66
LNP THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas..
Flexural Modulus >= 3.41 GPa
>= 495 ksi
ASTM D790
Buckeye Polymers BP RPP 3505 GM BLK Polypropylene, Glass Filled
Information Provided by Buckeye Polymers, Inc.