Mechanical Properties Metric English Comments
Flexural Modulus 3.48 GPa
505 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI
LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Flexural Modulus 3.48 GPa
505 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp DX99721 PC
LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 3.48 GPa
505 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp DX99721 PC (Asia Pacific)
LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.