Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD-[color]-H Nylon 66, 2% MoS2 Nylon 66, 2% Molybdenum Disulfide for Lubrication and Wear, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD1 Nylon 66, 1% MoS2 Nylon 66, 1% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD2 Nylon 66, 2% MoS2 Nylon 66, 2% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM-D790 |
Ineos ABS Lustran® SAN DN79 SAN Grade Lustran® SAN DN79 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for used in compounding. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | tangent; ASTM D790 |
Spartech PP5410 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES HiFill® PET GF15 IM 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790-07 |
3M Scotchkote™ 2400 Pipe Renewal Liner 3M Scotchkote Pipe Renewal Liner 2400 has been specifically developed for the rehabilitation of potable water pipe infrastructure to help extend service life, reduce leaks, and improve water quality.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790-07 |
3M Scotchkote™ 2400 Pipe Renewal Liner NSF/ANSI-61 certified polyurea formulation is 100% solids and contains no epoxy resin. It is designed to help solve a wide variety of problems common to potable water systems. It utilizes a trenchle.. |