Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 3.66 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.66 GPa
531 ksi
ASTM D 790
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer
Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn..
Flexural Modulus 3.66 GPa

@Temperature -40.0 °C
531 ksi

@Temperature -40.0 °F
ASTM D790
BASF Capron® 8200 NL Nylon 6 (Conditioned)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 3.66 GPa

@Temperature -40.0 °C
531 ksi

@Temperature -40.0 °F
ASTM D790
BASF Capron® 8202 NL Nylon 6 (Conditioned)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 3.66 GPa
531 ksi
15 mm/min; ASTM D790
LG Chemical 81HF SAN Resin
High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li..
Flexural Modulus 3.66 GPa
531 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EX06430H PEI
LNP* THERMOCOMP* EX06430H is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this grade is: Healthcare.
Flexural Modulus 3.66 GPa
531 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer
LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 3.66 GPa
531 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RZ006SXP PA 66
LNP* THERMOCOMP* RZ006SXP is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized.
Flexural Modulus 3.66 GPa
531 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RZ006SXP PA 66 (Asia Pacific)
LNP* Thermocomp* RZ006SXP is a compound based on Nylon 66 resin containing Milled Glass.
Flexural Modulus 3.66 GPa

@Temperature 300 °C
531 ksi

@Temperature 572 °F
ASTM D790
UBE UPIMOL® S High Heat Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..
Flexural Modulus 3.66 GPa
531 ksi
ASTM D790
Westlake Plastics PEEK Film Made from VICTREX® Polymer
Extremely high temperature resistance and continuous use temperature. Excellent flexural and tensile properties. Good abrasion and rain erosion resistance. Excellent chemical resistance. Excelle..
Flexural Modulus 3.66 GPa
531 ksi
ASTM Test
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.