Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 3.92 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
SABIC Innovative Plastics Cycoloy® MC5210 PC+ABS (Asia Pacific)
Flexural Modulus 3.92 GPa
569 ksi
DIN 53452; ASTM D790
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
SABIC Innovative Plastics Lexan® SP7602 PC (Asia Pacific)
Flexural Modulus 3.92 GPa

@Thickness 3.20 mm
569 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose
Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical
Flexural Modulus 3.92 GPa

@Thickness 3.20 mm
569 ksi

@Thickness 0.126 in
2.8mm/min; ASTM D790
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact
Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Flexural Modulus 3.92 GPa

@Thickness 3.20 mm
569 ksi

@Thickness 0.126 in
2.8mm/min; ASTM D790
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage
Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Flexural Modulus 3.92 GPa
569 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Flexural Modulus 3.92 GPa

@Thickness 3.20 mm
569 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance
Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical
Flexural Modulus 3.92 GPa
569 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN133MT40 M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 3.92 GPa
569 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC
LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release.
Flexural Modulus 3.92 GPa
569 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC
LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare.
Flexural Modulus 3.92 GPa
569 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC
LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 3.92 GPa
569 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC
LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific)
Flexural Modulus 3.92 GPa
569 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® VB-8102G MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
SABIC Innovative Plastics Xenoy® 1760 PBT+PC (Asia Pacific)
Flexural Modulus 3.92 GPa
569 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC
LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release
Flexural Modulus 3.92 GPa
569 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® VB-8102G MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 3.92 GPa
569 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6
Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a..
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
PlastxWorld CEVIAN® SERG1 10% GF ABS
Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
PlastxWorld CEVIAN® SKG10 10% GF ABS
Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast..
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
Flexural Modulus 3.92 GPa

@Thickness 6.40 mm
569 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IMG-1115 Glass Reinforced Grade
Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali
Flexural Modulus 3.92 GPa

@Thickness 6.40 mm
569 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IMG-1115 Glass Reinforced Grade
Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali
Flexural Modulus 3.92 GPa
569 ksi
Mitsui AURUM® JCR3030F Thermoplastic Polyimide Resin, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Modulus 3.92 GPa
569 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) ST60G3 Nylon 66, 15% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Modulus 3.92 GPa
568 ksi
ASTM D790
PlastxWorld CEVIAN® A5622 10% GF PA/ABS Alloy, DAM
Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
PlastxWorld CEVIAN® S5210 10% GF PC/ABS alloy
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld ..
Flexural Modulus 3.92 GPa
569 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific)
LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Copyright © lookpolymers.com All Rights Reserved