Mechanical Properties Metric English Comments
Flexural Modulus 0.210 GPa
30.5 ksi
1.7 mm/min; DIN 53457
Advanced Elastomer Systems VistaFlex® 911-B Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Flexural Modulus 0.210 - 13.1 GPa
30.5 - 1900 ksi
Average value: 2.42 GPa Grade Count:153
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
3M Dyneon™ THV 500A Fluorothermoplastic  (discontinued **)
THV 500A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of an agglomerate. As an agglomerate, it can be used for c..
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
Clariant Renol PBTSP0006 Polyester Elastomer
Data provided by Clariant Masterbatches
Flexural Modulus 0.210 GPa
30.5 ksi
Tangent Method 1; ASTM D-790
Bapolene® 1052 Polyethylene, Injection Grade
A medium flow general purpose injection molding resin with good gloss, toughness and good chemical resistance. This product meets FDA standards for food contact applications.Applications: Caps and ..
Flexural Modulus 0.210 GPa
30.5 ksi
Tangent Method 1; ASTM D-790
Bapolene® 1072 Polyethylene, Injection Grade
A high flow general purpose injection molding resin with good gloss, toughness and stress crack resistance. This product meets FDA standards for food contact applications.Applications: Housewares, ..
Flexural Modulus 0.210 GPa

@Temperature 93.0 °C
30.5 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8350 HS PA6 (Dry)
Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate..
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
3M Dyneon™ THV 500GZ Fluorothermoplastic Granules
THV 500G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature proce..
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
Ashley Polymers Ashlene® ABS 220
High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the m..
Flexural Modulus 0.210 GPa
30.5 ksi
ASTM D790
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc  (discontinued **)