Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.075 GPa | 301.0 ksi | ISO 178 |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Flexural Modulus | 2.075 GPa | 301.0 ksi | DIN 53452 |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |