Polymer Property : Flexural Modulus = 309.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.136 GPa
309.8 ksi
ASTM D 790
MRC Polymers NAXALOYâ„¢ 793A7 PC + Polyester Blend
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Flexural Modulus 2.136 GPa

@Thickness 3.17 mm
309.8 ksi

@Thickness 0.125 in
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ABS TS-12 Injection Molding Grade, Medium Heat
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.136 GPa
309.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ASA S-170 Lt Grey 50283UV f1 ASA Weatherable Polymers Injection Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.