Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 31.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.220 GPa
31.9 ksi
ISO 178
Polimeri Europa Flexirene® MT 40 A Linear Low Density Polyethylene
Flexirene MT 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Flexirene MT 40 A is characterized by a good processability and impact r..
Flexural Modulus 0.220 - 9.31 GPa
31.9 - 1350 ksi
Average value: 2.85 GPa Grade Count:307
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Modulus 0.220 GPa
31.9 ksi
ASTM D790
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium  (discontinued **)
Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Flexural Modulus 0.220 GPa
31.9 ksi
ISO 178
Metabolix M-veraâ„¢ B5010 Film Grade Compostable Bioplastic
For use in tough, certified compostable film and bag applications. Mvera B5010 offers a wide range of attractive traits—excellent tear and puncture toughness, excellent seal strength, good prin..
Flexural Modulus 0.220 GPa
31.9 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer
LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant.
Flexural Modulus 0.220 GPa
31.9 ksi
ASTM D790
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 15 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Flexural Modulus 0.220 GPa
31.9 ksi
ASTM D790
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls
DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig..
Flexural Modulus 0.220 GPa
31.9 ksi
ASTM D790
DuPont™ Surlyn® 9650 Ionomer Resin, Zinc
Surlyn® 9650 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Flexural Modulus 0.220 GPa
31.9 ksi
SAE J949
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.220 GPa

@Temperature 93.0 °C
31.9 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® HPN 9350 HS PA6 (Dry)
Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res..
Flexural Modulus 0.220 GPa
31.9 ksi
ISO 178
Teknor Apex Sinvicomp DFR 5806 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex