Polymer Property : Flexural Modulus = 3101 ksi
Polymer Property :
Flexural Modulus =
3101 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
21.38
GPa
3101
ksi
ASTM D-790
PlastiComp Complet® LCF30/LGF20 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber
Composite PelletsInformation provided by PlastiComp, Inc.