Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.175 GPa | 315.5 ksi | |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |