Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.19 GPa | 317 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4000HH Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.19 GPa | 317 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4000HH-ELG Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc. |