Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.19 GPa | 318 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | Tangent (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 3514 Description: Black Polycarbonate Polyester AlloyInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL TCN8222 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled 80C FR-V2 |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | ISO 178 |
Polyram RamTough PZ509 Polycarbonate, Easy Flow, Flame Retardant Non-transparent polycarbonate, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | ISO 178 |
Polyram RamTough PZ513 Polycarbonate, Easy Flow, Flame Retardant Transparent polycarbonate, UV stabilized, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.19 GPa | 317 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4000HH Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.19 GPa | 317 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4000HH-ELG Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.19 GPa | 318 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |