Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.234 GPa | 33.9 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 4502 BLK Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo.. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 2% Secant, 12.7 mm/min; ASTM D790 |
Eastman D4027-P Voridian Polyethylene
(discontinued **) VORIDIAN low density polyethylene D4027-P is a formulation suggested for extrusion coating applications that require clarity, high gloss and superior hot tack properties. Applications/UsesFood Packa.. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 - 45.0 GPa | 33.9 - 6530 ksi | Average value: 9.38 GPa Grade Count:74 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |