Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.400 GPa | 348.1 ksi | 1% tangent, 0.05 in/min.; LAB033 |
ExxonMobil Mytex™ AS65KW-1ATM Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical |
|||
Flexural Modulus | 2.400 GPa | 348.1 ksi | 1% tangent, 0.05 in/min.; LAB033 |
ExxonMobil Mytex™ AS65KW-LGDC Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical |