Polymer Property : Flexural Modulus = 370 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.196 - 2.55 GPa
28.4 - 370 ksi
Average value: 2.06 GPa Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Flexural Modulus 2.24 - 2.55 GPa
325 - 370 ksi
ASTM D790
Alcoa KAMA 4100 Prime APET  (discontinued **)
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,..
Flexural Modulus 2.24 - 2.55 GPa
325 - 370 ksi
ASTM D790
Alcoa KAMA 4200 RPET  (discontinued **)
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled..
Flexural Modulus 2.24 - 2.55 GPa
325 - 370 ksi
ASTM D790
Alcoa KAMA Petwich-PET 4300 Petwich-PET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi..
Flexural Modulus 2.24 - 2.55 GPa
325 - 370 ksi
ASTM D790
Alcoa KAMA 4203 Impact Modified RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a..
Flexural Modulus 2.41 - 2.55 GPa
350 - 370 ksi
ASTM D790
Alcoa KAMA SealPET™ 4205 RF Sealable RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a..
Flexural Modulus 2.41 - 2.55 GPa
350 - 370 ksi
ASTM D790
Alcoa KAMA 4223 Impact Modified RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl..