Mechanical Properties Metric English Comments
Flexural Modulus 26.0 GPa
3770 ksi
Lehmann & Voss LUVOCOM® 20/XCF/30 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Flexural Modulus 26.0 GPa
3770 ksi
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 26.0 GPa
3770 ksi
ISO 178
Vyncolit X659 Glass, Mineral and Graphite Filled Novolac Phenolic
Novolac resin based, glass fiber, mineral and graphite filled. Grade with superior stiffness, high dimensional stability and excellent tribological properties. Good chemical resistance against sever..