Mechanical Properties Metric English Comments
Flexural Modulus 0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips KN 226B LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode..
Flexural Modulus 0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips KN 230 LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware..
Flexural Modulus 0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips KN 230B LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ..
Flexural Modulus 0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips Marlex® 1409 Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications..
Flexural Modulus 0.269 GPa
39.0 ksi
2% Secant, 12.7 mm/min; ASTM D790
Eastman 1840A Polyethylene  (discontinued **)
Polyethylene 1840A is a low-density formulation with no slip or antiblock. It is suggested for injection molding applications requiring good stiffness, gloss, good processability or layflat properti..
Flexural Modulus 0.269 GPa
39.0 ksi
2% Secant, 12.7 mm/min; ASTM D790
Eastman 1840E Polyethylene  (discontinued **)
Polyethylene 1840E is a low-density formulation for general extrusion.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer app..
Flexural Modulus 0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips Marlex® 1412 Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications..
Flexural Modulus 0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware..
Flexural Modulus 0.269 GPa
39.0 ksi
Dow LDPE 955I Low Density Polyethylene