Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 1412 Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 1412 Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications:Lids and Over-Caps using Multilevel MoldsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 11.1 MPa
1610 psi
ASTM D638
Tensile Strength, Yield 11.1 MPa
1610 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 0.193 GPa
28.0 ksi
3 pt. secant; ASTM D790
0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Brittleness Temperature -38.0 °C
-36.4 °F
ASTM D746
Users viewing this material also viewed the following: