Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.01 GPa | 582 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |
|||
Flexural Modulus | 4.01 GPa | 582 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |