Mechanical Properties Metric English Comments
Flexural Modulus 4.01 GPa
582 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® 1760E PBT+PC
11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin.
Flexural Modulus 4.01 GPa
582 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC
LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.