Mechanical Properties Metric English Comments
Flexural Modulus 0.0277 GPa
4.02 ksi
ASTM D790
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat..