Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.36 GPa | 632 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Flexural Modulus | 4.36 GPa | 632 ksi | ISO 178 |
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |