Polymer Property : Flexural Modulus = 632 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.36 GPa
632 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT
LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber.
Flexural Modulus 4.36 GPa
632 ksi
ISO 178
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..