Flexural Modulus 4.39 GPa
637 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
Flexural Modulus 4.39 GPa
637 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT (Asia Pacific)
LNP* Lubricomp* WAL34 is a compound based on Polybutylene Terephalate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
Flexural Modulus 4.39 GPa
637 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP
LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral.
Flexural Modulus 4.39 GPa
637 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific)
This material is mineral filled PPO grade with high dielectric constant and low loss tangent
Flexural Modulus 4.39 GPa
637 ksi
ISO 178
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba..
Flexural Modulus 4.39 GPa
637 ksi
ISO Data
BASF Ultramid® TG3S BK-104 15% Glass Filled PA6 (Dry)
Ultramid TG3S BK-104 is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a balance ..