Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.56 GPa | 661 ksi | ASTM D790 |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 4.56 GPa | 661 ksi | ASTM D790 |
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |