Polymer Property : Flexural Modulus = 661 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.56 GPa
661 ksi
ASTM D790
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 4.56 GPa
661 ksi
ASTM D790
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).