Polymer Property : Flexural Modulus = 4.73 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.73 GPa
686 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (Cond)
Information provided by Ravago.
Flexural Modulus 4.73 GPa
686 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N2040MGL Nylon 6 (Cond)
Information provided by Ravago.