Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
DAM; ASTM D792
Water Absorption 0.90 %
0.90 %
24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
0.125 in, DAM; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 4.73 GPa
686 ksi
ASTM D790
Processing Properties Metric English Comments
Melt Temperature 260 - 282 °C
500 - 540 °F
Mold Temperature 71.1 - 98.9 °C
160 - 210 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.18 %
0.18 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 50 - 120 rpm
50 - 120 rpm