Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.94 GPa | 716 ksi | ASTM Test |
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-106 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Flexural Modulus | 4.94 GPa | 716 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |