Polymer Property : Flexural Modulus = 716 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.94 GPa
716 ksi
ASTM Test
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS BK-106 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..
Flexural Modulus 4.94 GPa
716 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp FF006 PE
LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region.