Mechanical Properties Metric English Comments
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid)
Interior application for thick & thin gauge profile application.Information provided by PolyOne
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6
LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin.
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 (Asia Pacific)
LNP* Colorcomp* PX99848 is a compound based on Nylon 6 resin containing Unfilled Custom Color.
Flexural Modulus 2.88 GPa
418 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Flexural Modulus 2.88 GPa
418 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66
LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Flexural Modulus 2.88 GPa
418 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DD0009 PC
LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.88 GPa
418 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.88 GPa
418 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.88 GPa
418 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific)
LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*..
Flexural Modulus 2.88 GPa
418 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp 4X08423
LNP* Thermocomp* 4X08423 is a compound based on Perfluoroalkoxy Polymer (PFA) containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
Teknor Apex APEX® RE 9016A Polyvinyl Chloride, Rigid
Features: Good Weather Resistance; High Impact Resistance Forms: PelletsInformation Provided by Teknor Apex
Flexural Modulus 2.88 GPa
418 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA 91802
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.88 GPa
418 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.