Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 29.31 GPa
4251 ksi
ASTM D-790
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Flexural Modulus 29.31 GPa
4251 ksi
ASTM D-790
PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.