Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 29.6 GPa @Temperature 23.9 °C |
4300 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Flexural Modulus | 29.65 GPa | 4300 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LX09404 PEEK LNP* THERMOCOMP* LX09404 is a compound based on Polyetheretherketone resin containing Carbon Fiber. |