Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced

Category Polymer , Thermoset , Epoxy
Manufacturer Park Electrochemical Corp.
Trade Name Nelcote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system for sandwich panel applicationsFlame retardant and self-extinguishingLow tack and long out-times for ease of processingApplications/Qualifications:Sandwich panels / structuresAircraft InteriorsMass Transit InteriorsInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Volatiles <= 1.0 %

@Temperature 163 °C
<= 1.0 %

@Temperature 325 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 483 MPa

@Temperature 23.9 °C
70000 psi

@Temperature 75.0 °F
ASTM D638
Tensile Modulus 26.2 GPa

@Temperature 23.9 °C
3800 ksi

@Temperature 75.0 °F
Dry; ASTM D638
Flexural Strength 758 MPa

@Temperature 23.9 °C
110000 psi

@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 29.6 GPa

@Temperature 23.9 °C
4300 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Compressive Strength 579 MPa

@Temperature 23.9 °C
84000 psi

@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus 24.1 GPa

@Temperature 23.9 °C
3500 ksi

@Temperature 75.0 °F
Dry; ASTM D695
Shear Strength 59.3 MPa

@Temperature 23.9 °C
8600 psi

@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 93.0 °C
199 °F
Dry; DMA
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Climbing Drum Peel (in-lb/3in) 45
ASTM D1781; Bag Surface
50
ASTM D1781; Mold Surface
Fabric Area Weight (g/m²) 300
Prepreg Resin Content (%) 37-43
Resin Flow (%) 10-25
275°F, 15psi
Users viewing this material also viewed the following: