Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.003 GPa | 435.5 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |