Polymer Property : Flexural Modulus = 435.55 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.0030 GPa
435.55 ksi
ASTM D790
Westlake Plastics HTP 800 Clear PVC
HTP 800 is a clear PVC based material for use as windows and doors in cleanroom equipment. Notable properties include light transmission, chemical resistance, and flame resistance. Information prov..