Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.552 - 30.0 GPa | 80.0 - 4350 ksi | Average value: 16.1 GPa Grade Count:29 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Flexural Modulus | 0.686465 - 30.0 GPa @Temperature 150 - 260 °C |
99.5649 - 4350 ksi @Temperature 302 - 500 °F |
Average value: 6.87 GPa Grade Count:28 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |