Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.65 - 5.03 GPa | 530 - 730 ksi | |
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Flexural Modulus | 3.65 - 5.03 GPa | 530 - 730 ksi | |
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |