Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 730 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.65 - 5.03 GPa
530 - 730 ksi
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound
BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
Flexural Modulus 3.65 - 5.03 GPa
530 - 730 ksi
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound
BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..