Mechanical Properties Metric English Comments
Flexural Modulus 5.28 GPa
766 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific)
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Flexural Modulus 5.28 GPa
766 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66
LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
Flexural Modulus 5.28 GPa
766 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.