Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.28 GPa | 766 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific) LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 5.28 GPa | 766 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66 LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 5.28 GPa | 766 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |