Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.515 - 6.895 GPa | 799.9 - 1000 ksi | ASTM D790 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |